AbstractAn attempt was made for the effective utilization of iron ore slime in making of geopolymer mortar along with other industrial wastes fly ash and LD-slag and achieved the appreciable compressive strength results with 8 M NaOH after 28 days at a curing period of 24 h at 55°C.  Keywords: Fly ash, LD-slag, geopolymer, compressive strength, NaOH, iron ore slimeCite this Article  Rajesh Chintala, R.K. Rath, Anil Kumar. Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar. Recent Trends in Civil Engineering & Technology. 2017; 7(1): 9–16p.