Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar

作者

  • Rajesh Chintala
  • R. K. Rath
  • Anil Kumar

##semicolon##

Fly Ash##common.commaListSeparator## LD-Slag##common.commaListSeparator## Geopolymer##common.commaListSeparator## Compressive Strength##common.commaListSeparator## NaOH##common.commaListSeparator## Iron ore Slime

摘要

AbstractAn attempt was made for the effective utilization of iron ore slime in making of geopolymer mortar along with other industrial wastes fly ash and LD-slag and achieved the appreciable compressive strength results with 8 M NaOH after 28 days at a curing period of 24 h at 55°C.  Keywords: Fly ash, LD-slag, geopolymer, compressive strength, NaOH, iron ore slimeCite this Article  Rajesh Chintala, R.K. Rath, Anil Kumar. Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar. Recent Trends in Civil Engineering & Technology. 2017; 7(1): 9–16p.

出版日期

2017-04-21

期號

分類

Research Articles